活性炭负载二氧化钛改性聚丙烯熔喷无纺布的制备及吸附性能
作者:
作者单位:

1.航天特种材料及工艺技术研究所,北京,100074;2.河南工程学院材料与化学工程学院,郑州,450000;3.空军装备部驻北京地区第二军事代表室,北京,100074

作者简介:

通讯作者:

孟庆杰,女,博士,高级工程师,E-mail:12312166@qq.com。

中图分类号:

O643

基金项目:


Preparation and Adsorption of Titanium Dioxide/Activated Carbon/Polyproylene Nonwovens by Melt Blown Method
Author:
Affiliation:

1.Aerospace Special Materials and Processing Technology Institute, Beijing, 100074, China;2.Department of Material and Chemical Engineering, Henan University of Engineering, Zhengzhou, 450000, China;3.The Second Military Representative Office of Air Force Equipment Department in Beijing, Beijing, 100074, China

Fund Project:

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    将活性炭、二氧化钛、聚丙烯等原料经物理共混处理,通过熔喷制成活性炭负载二氧化钛改性聚丙烯熔喷无纺布。采用热分析曲线(Differential scanning calorimeter, DSC)、X射线衍射(X-ray diffraction, XRD)、电子织物拉伸机、可见分光光度计等对改性无纺布的微观结构、结晶性能、力学性能、吸附性能进行表征。结果表明:活性炭负载二氧化钛比例为1∶3时活性炭负载二氧化钛的降解率高,二氧化钛分布均匀,依照此比例的活性炭负载二氧化钛与聚丙烯进行熔喷制备无纺布。随活性炭负载二氧化钛的加入量的提高,活性炭负载二氧化钛改性聚丙烯无纺布的吸附性能增强,当活性炭负载二氧化钛的添加量为4%时,吸附性能较好;活性炭负载二氧化钛的添加使无纺布的力学性能出现最大值,且无纺布的结晶度和熔点无明显变化。

    Abstract:

    Activated carbon/TiO2/polypropylene(PP) non-wovens were prepared by physical blending of activated carbon/TiO2/PP. The microstructure, crystalline properties, mechanical properties and adsorption properties of PP nonwovens were characterized by differential scanning calorimeter (DSC), X-ray diffraction (XRD), electronic fabric stretching machine and visible spectrophotometer. The experimental results show that the degradation rate of TiO2 supported on activated carbon is high and the distribution of TiO2 is uniform when the ratio of activated carbon to titanium dioxide is 1∶3, so the ratio of activated carbon / TiO2 and PP is used to prepare non-woven fabrics by melt spraying. Therefore, the 1∶3 ratio of activated carbon/TiO2 to PP is used to melt-blown the nonwoven fabric. With the increase of the amount of activated carbon/TiO2, the adsorption performance of activated carbon/TiO2/PP non-woven fabrics is enhanced. When the amount of activated carbon loaded titanium dioxide is 4%, the adsorption performance is better; the addition of activated carbon/TiO2 made mechanical properties of the non-woven fabrics reach the maximum value, but it has little effect on the crystallinity and melting point of the non-woven fabrics.

    参考文献
    相似文献
    引证文献
引用本文

孟庆杰,兰天,李南,迟长龙,孙波.活性炭负载二氧化钛改性聚丙烯熔喷无纺布的制备及吸附性能[J].南京航空航天大学学报,2019,51(6):857-863

复制
分享
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:2018-12-10
  • 最后修改日期:2019-02-27
  • 录用日期:
  • 在线发布日期: 2020-01-06
  • 出版日期:
文章二维码
您是第位访问者
网站版权 © 南京航空航天大学学报
技术支持:北京勤云科技发展有限公司